N07752 Nickel Base Superalloy Plate Coil Plate Bar Pipe Fitting Flange Square Tube Round ...
Product Introduction
Since the establishment of the company, we have accumulated a wealth of professional manufacturing technology and valuable experience through long-term research and exploration of Tungsten Rhenium Alloy Wire, Pure Iridium Foil, Zr 702 Zirconium Tube. We have a complete after-sales service team to provide you with one-stop service to solve your worries. The company insists on seeking development through innovation, and has established a high-tech product research and development center with a group of high-quality professionals. At our company, we treat each other with respect and equality at all times - just as we would like others to treat us. We firmly believe that extremely high product cost performance is the foundation of the company's sustainable development. With the rapid development since its inception our company has served to a great majority of customers through continuous innovation philosophy and pre-market awareness.
Nickel Pipe Fittings
FANMETAL supply the Ni200 Nickel Pipe fittings according to ASME B16.9. Such as nickel tee, nickel threadolet, nickel reducer, nickel end cap, nickel elbow, nickel collar etc. Material nickel 200 ( UNS N02200 ) and nickel 201 ( UNS N02211 )
Ni200 Nickel Pipe fittings Specification:
Dimensions ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79
Size 1/8” NB TO 48” NB. (Seamless & 100% X-Ray Welded, Fabricated)
Type Seamless / Welded / Fabricated
Bending Radius R=1D, 2D, 3D, 5D, 6D, 8D, 10D or Custom
Thickness Sch 5s, Sch 10s, Sch 40s, Sch 80s, Sch 160s, Sch XXS
Grade Hastelloy C276 Pipe Fittings UNS (N10276), DIN (2.4819)
Nickel Pipe Fittings Picture:



Nickel 200 alloy is a commercially pure nickel that exhibits
good corrosion resistance. It is ferromagnetic and has relatively low
electrical resistivity. This combinationof properties has allowed its use in a wide variety of applications.
Nickel 201 alloy is a low carbon modification
Nickel 200 alloy that has found applications in the electronic industry at temperatures up to 1200°F(649°C). It is preferred to Nickel 200 alloy above 600°F(315°C), because of
its better resistance to "creep."
The quality of our N07752 Nickel Base Superalloy Plate Coil Plate Bar Pipe Fitting Flange Square Tube Round ... has been well received by users over the years. We achieve innovation-driven, transformational development. We are committed to building harmonious labor relations, allowing the company to develop continuously and healthily, so that employees and the company can grow together.
Hot Tags: Nickel Pipe Fittings, suppliers, manufacturers, factory, customized, wholesale, price, quotation, for sale, Tungsten Precision Mold, Molybdenum Mo Electrode, Inconel 625 Alloy Flange, Pure 99 999 Titanium Sputtering Target, Stellite 6K knife, tantalum fasteners
[[ProKeywords]]SPEC DATA